MEMSnet Home: MEMS-Talk: The Temperature of DRIE
The Temperature of DRIE
2002-08-12
Madanagopal K.V.
The Temperature of DRIE
Madanagopal K.V.
2002-08-12
Hi!
The wafer temperature can climb till about 60C for thru wafer etches.

Madan


At 08:20 PM 5/15/2002 +0800, you wrote:
>Who knows the temperature in DRIE when silicon is deep-etched, say 500microns?
>
>Thanks.
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/

___________________________________________________________

K.V.Madanagopal, Ph.D.
Senior Research Associate
Alliance for Nanomedical Technologies
317 Stocking Hall
Cornell University
Ithaca
NY 14850
Fax:607-255-8741
Phone:607-254-8052
___________________________________________________________

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.