Hi,

Try Technics Inc in Cranston RI    Tel # is 401-781-6100


Rick


Rick Morrison
Sr. Semiconductor Engineer
Radant Mems Inc.
255 Hudson Road
Stow Ma, 01775
Tel- 978-562-3866
Cell 508-801-4796
AMS Phone: 508-770-3521
EMAIL  [email protected]