evaporation on plastic
SP
2002-08-14
I've used an Ar plasma etch of Mylar and other materials in situ with good
results. The
subsequent thermal deposition of Au (1000A) adhered very well.

                                                                          Steve




At 11:08 PM 8/13/02 -0700, you wrote:
>Dear MEMS community:
>
>I want to put gold on some plastic substrate by
>evaporation, either thermal or e-beam. Does any one
>know which kind of plastic can survive for this
>application. BTW, how to clean plastic wafers?
>Any comments is appreciated.
>
>Lisen
>HotJobs - Search Thousands of New Jobs
>http://www.hotjobs.com
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/







----------
Visit our Web site at <www.formatrix.com>ban1.jpg
PH: 408-980-9324
FAX: 408-980-9326

[demime 0.98e removed an attachment of type image/jpeg which had a name of
ban1.jpg; x-mac-type=4A504547; x-mac-creator=4A565752]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.