MEMSnet Home: MEMS-Talk: CVD deposition of metal needed !
CVD deposition of metal needed !
2002-08-15
Frank Rasmussen
2002-08-15
Neal Ricks
2002-08-15
[email protected]
2002-08-16
Bill Moffat
CVD deposition of metal needed !
[email protected]
2002-08-15
I hope you mean you want to deposit metals via Physical Vapor Deposition (PVD)
Sputtering of the metals you listed is readily accomplished in the
temperature ranges you suggest. Try www.thinfilmsinc.com for a foundry to do
your work. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing