MEMSnet Home: MEMS-Talk: Re: about crosslinking PMMA
Re: about crosslinking PMMA
2002-08-21
Tatiana Borzenko
Re: Laser Printer Masks
2002-08-21
Craig McGray
Re: about crosslinking PMMA
Tatiana Borzenko
2002-08-21
Dear colleague,
if you need to cross-link PMMA as a film you can find my information useful.
PMMA starts to crosslink under high dose of actinic irradiation. For
example, being well known as the high resolution positive electron
resist it behaves in this way till the electron dose does not exceed
approximately (1-5)*10^(-3)C/cm^2. This dose value, when crosslinking in
PMMA starts to appear, depends on the voltage, the substrate and the
film thickness. At doses about 10^(-1)C/cm^2 the PMMA film is
practically not solved in all PMMA developers.
The idea to use PMMA as a negative resist is not nice. It will have low
contrast  and it is not possible to dissolve it in solvents usually used
in microfabrication if it needs to be removed. But it can be easily
removed in O-plasma.  PMMA film, when crosslinked, can serve as an
insulating layer in some laboratory micro- or nano-devices. Which
irradiation to use (UV- or electron) depends on the film thickness. UV
does not penetrate deep. At crosslinking the film thickness shrinks
because low volatile products which are formed during irradiation leave
the polymer.
Sincerely, T.Borzenko.
___________________________________________________________________________
Dr.T.Borzenko
EP3
Physikalisches Institut der Universitaet Wuerzburg
Am Hubland 97074 Wuerzburg
Deutschland
tel +49 931 8885876
fax +49 931 8885142
e-mail:    [email protected]


___________________________________________________________________________

Original message:

>Message: 2
>From: "Emer O'Reilly" 
>To: 
>Date: Tue, 20 Aug 2002 17:38:48 +0100
>Subject: [mems-talk] crosslinking PMMA
>Reply-To: [email protected]

>Dear all,

>Would anyone be able to direct me towards some information please: I wish >to
>find out how to cross link PMMA.

>Thanks in advance.

>Emer.


***********************************************************************
>Research Engineer, Nanotechnology Group,
>NMRC, University College, CORK.
>Ireland

>Direct line: +353 (0)21 4904182
>Fax: +353 (0) 21 4270271
>http://www.nmrc.ie/research/nanotechnology-group/index.html
***********************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer