MEMSnet Home: MEMS-Talk: Flat Wire
su-8 2100 resist problems
2002-08-22
dav ng
Flat Wire
2002-08-22
RobDavis
Flat Wire
RobDavis
2002-08-22
Howdy,

Looking for flat wire to make contact with die pad.  Want it to be ~ 1mm
wide and maybe 50 micron thick.  Want it to be a nickel alloy or
copper-nickel....

Web search have found one or two suppliers overseas....all want huge orders

If all fails I will cut foil to make the interconnect.

Any comments?
Thanks

Rob