Rob,

Try ordering a sample from MWS Wire Industries (www.mwswire.com).  I know
they have copper flat wire but not sure about the nickel plate.  If they
don't have it plated it is easy to plate the copper flat wire yourself in a
small quantity.

Harold L. Snyder, Jr.
Scientist & Consultant

Begin Included Message:
==========================
Subj:   [mems-talk] Flat Wire
Date:   8/22/2002 11:40:30 AM Central Daylight Time
From:   [email protected]
Reply-to:   [email protected]
To: [email protected]
Sent from the Internet (Details)


Howdy,

Looking for flat wire to make contact with die pad.  Want it to be ~ 1mm
wide and maybe 50 micron thick.  Want it to be a nickel alloy or
copper-nickel....

Web search have found one or two suppliers overseas....all want huge orders

If all fails I will cut foil to make the interconnect.

Any comments?
Thanks

Rob

==========================
End Included Message.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
Harrick Plasma, Inc.