Hello everyone,

I wonder if any readers could offer their advice on the following requirement:

  BPSG deposition at >> 280 angstroms/minute, with ~10% wafer-to-wafer thickness
  uniformity and ~5% within-wafer thickness uniformity on batches of 50 100mm
  wafers.

Any opinions or pointers on how this might be or is being done?

With Regards,

Cam Sorlie


____________________________________________________________________________
                             Box 1932 Main Station         T: 1 403 435 2167
Cameron Sorlie, President    Edmonton, AB T5J 2P3 Canada   F: 1 403 433 9376
General Microdevices, Inc.   -----------------------------------------------
                             [email protected]
______________________________________________________
     Microtechnology products for science and industry


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.