Several months ago I asked members about a Decon Dalo resist pen.
This pen writes a thick resist that holds up pretty well to plasma etches and
several acids,
but is readily removed with acetone or resist stripper.
We have found it handy for doing quick etching tests.

Thanks to those who replied. I finally found a U.S. supplier.
Many people had asked for ordering information. Here it is:

The pens are manufactured by ITW Dymon in Olathe, Kansas, USA.
ITW Dymon does not, however, sell the pens directly.

A retail distributor that sells them in the U.S. is McMaster-Carr in Santa Fe
Springs, California, USA,
See www.mcmaster.com or call (562) 692-5911.
They are sold on lots of 24 for about $4 each.
They must be special ordered as they not part of their regular inventory.
Due to this, it may take some convinicing to find someone willing to take your
order.
The U.S.-sold pens say "ACTION MARKER Fine Line 33 PC-901 BLUE" on them.
McMaster-Carr knows them as "ITW #33901, DALO PC BLUE 33 PEN" Part Number 16305
T999.

In the U.K., Decon Laboratories adds its name to the pens, with the label
"Decon-Dalo 33 Blue PC."
See www.decon.co.uk.

*****************************************
Kirt R. Williams, Ph.D., P.E.
Member of Technical Staff
Electronics Research Laboratory

Agilent Technologies, Inc.
3500 Deer Creek Road, MS 26M2
Palo Alto, CA  94304  USA

+1 (650) 485-3562 Tel
+1 (650) 485-8626 Fax
[email protected]
www.agilent.com
*****************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.
MEMS Technology Review