        HI Xu,
        I think the machine you are referring to is call a Goniometer  the
company that make them is:
        Raime-Hart, Inc.
        43 Bloomfield Ave.
        Mountain Lake, N.J., U.S.A.
        telephone # (201) 335-0560
        regards,
        Ed Knighton, Process Engineeer,

> -----Original Message-----
> From: Xu, Junquan [SMTP:[email protected]]
> Sent: Friday, August 23, 2002 8:30 PM
> To:   '[email protected]'
> Subject:      [mems-talk] contact angle
>
> Hi all,
>
> Do you know which company sell the machine for contact angle measurement?
>
> regards,
>
> Junquan Xu
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review