Sungjun Lee
2002-09-04
W.H. Teh
lift off problem
Sungjun Lee
2002-09-03
Does anyone who knows about the lift-off of PMMA?
I have usually done it under boiling Acetone.
Is there any difference of behavior under between pure Acetone and boiling?
By the way, I welcom to receive any comment about the lift off method.
Thanks in advance.