MEMSnet Home: MEMS-Talk: Wet etching of Germanium
Wet etching of Germanium
2002-09-10
Jean-jacques Simon
2002-09-10
[email protected]
Wet etching of Germanium
Jean-jacques Simon
2002-09-10
Dear all mems-talk members,

I m looking for a wet etching solution in order to etch Germanium?

Can someone give me an advice or references?

Thanks for your kindness

Doctor Jean-Jacques SIMON
Maître de Conférences
Institut Fresnel / COM
Dom. Univ.de St Jérôme
13397 Marseille cedex 20 France
tel. 33 4 91 28 80 66
fax 33 4 91 28 80 67
email : [email protected]




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing