MEMSnet Home: MEMS-Talk: Etching of gaas native oxide
Etching of gaas native oxide
2002-09-10
Fabio Altomare
2002-09-11
Robert C Cole
2002-09-11
Fabio Altomare
Etching of gaas native oxide
Robert C Cole
2002-09-11
I believe a 10 % solution of HCl will etch the native oxide on GaAs.

Bob Cole
The Aerospace Corporation




reply