MEMSnet Home: MEMS-Talk: Wafer cleaning
Wafer cleaning
2002-09-13
Soojin Oh
2002-09-13
Justin Borski
Wafer cleaning
Soojin Oh
2002-09-13
For vacuum evaporation, how do you clean your wafers?
What I did was several baths of organic solvents
(Acetone, MeOH, EtOH) and water followed by UV-Ozone,
and finally "Piranha" bath cleaning. Finally I rinse
wafers in DI water and blow dry w/ N2 gas. But after
metal deposition I can still see some particular
impurities apparently imbedded underneath. What should
I do? Thank you for any suggestions and advices.

-Soojin
UNC-CH



__________________________________________________
Do you Yahoo!?
Yahoo! News - Today's headlines
http://news.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing