Hi,
What material is your substrate?
You are cleaning for organics and inorganics, but not particulates. You could
try someting like
SC1 with H20,NH3,and H2O2 for particulate removal.

Lakshmi Namburi.
Teravicta Technologies, Austin,TX.

__________________________________________________
Do you Yahoo!?
Yahoo! News - Today's headlines
http://news.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review