info about elastomer sheets
[email protected]
2002-09-18
Bernard,

Take a look at PORON (www.rogerscorporation.com/hpf/CT/).  It is available in
both closed cell and open cell.  You should be able to get samples from a
local distributor.

Harold L. Snyder, Jr.
Scientist & Consultant

Begin Included Message:
===========================

> Subj:[mems-talk] info about elastomer sheets
> Date:9/12/2002 1:55:14 PM Central Daylight Time
> From:bernard-
[email protected]
> Reply-to:[email protected]
> To:[email protected]
> Sent from the Internet
>
>
>
> Hi,
>
> I am looking for thin (100-200 micron) elastomer
> sheets and would be grateful for any info
> about possible suppliers.
>
> Thanks!
>
> --
> Bernard Bunner, Ph.D.
> Senior Engineer
> Teragenics
> 80 Rosedale
> Watertown, MA 02472
> phone: 617-926-0877 ext 246
> fax: 617-926-0878
> email: [email protected]
>
>
>

===========================
End Included Message.









reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
Harrick Plasma, Inc.