A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Si wafers with special surface orientation
Si wafers with special surface orientation
2002-09-19
Matthias Heschel
2002-09-19
David Nemeth
2002-09-19
bille@npphotonics (Bill Eaton)
2002-09-20
Kenneth Smith
2002-09-19
[email protected]
2002-09-19
[email protected]
Si wafers with special surface orientation
Kenneth Smith
2002-09-20
Daer Dr. Heschel,

I often have customers that are in need of specific off angle silicon
silices and we are able to process to virtually any range desired
including 9 degree with fairly tight tolerances.

Although I do not handle etching cavities and I could be mistaken, I
have process a number of requests for a 9.7 degree off angle that users
suggest is best for the 45 degree sidewall.

Please contact me via email or other- off list to follow up on your
request.

Best Regards,
Ken Smith

Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510-217-4421 or 561-658-6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.Quartz, Glass, Pyrex
and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.


Matthias Heschel wrote:

> I am trying to get 45° side wall angles in KOH etched cavities (silicon
substrates). I am aware of some etching work that has been performed on 100 Si
wafers. I am rather looking for wafers that are sawn in a 9° angle respective to
100. I found several sources for different angles, which are unfortunately too
far away from my 9°. Does anybody have wafers with an angle close to 9° or know
of a potential supplier? Any response is very much appreciated.
>
> *************************************************************************
> Matthias Heschel, PhD
> VP Engineering
>
> Hymite ApS, DTU, Bldg. 325, 1st floor
> 2800 Kgs. Lygnby, Denmark
>
> Direct: +45 45259155
> Cell: +45 22723365
> Fax: +45 45259156
>
> Email: [email protected]
> http://www.hymite.com
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>


--




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.