MEMSnet Home: MEMS-Talk: Gold etchant without attacking ZnO
Gold etchant without attacking ZnO
2002-09-25
hongyu
Gold etchant without attacking ZnO
hongyu
2002-09-25
Hi, friends

I wnat to etch Gold, but my gold is on ZnO. Is there anyone knows that what kind
of  Gold etchant will not attack ZnO?
Thanks a lot
Hongyu