PECVD nitride/oxide layer as a mask for KOH silicon etching
2002-10-03
Swiss Chen
PECVD nitride/oxide layer as a mask for KOH silicon etching
Swiss Chen
2002-10-03
Can I use PECVD nitride or oxide layre as a mask for KOH silicon etching? I
just want to etch 10-20um on silicon. Could someone tell me if this works
fine? And also I am not sure if the KOH will attach Au/Cr layer.

Thanks,

Swiss


_________________________________________________________________
Chat with friends online, try MSN Messenger: http://messenger.msn.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering