Dear Rahul

I see that you are sputtering SnO2. I am interested in this and wonder
if you have any references. Are you reactively sputtering from an Sn
target in Ar/O2 atmosphere, or are you sputtering from a Sn target?


Regards


Richard Haigh

-----Original Message-----
From: Mr. Rahul Mishra [mailto:[email protected]]
Sent: 03 October 2002 17:01
To: Vijaykumar G
Cc: [email protected]
Subject: [mems-talk] SnO2 Etchant

Hi
Can anybody tell me the etchant for Sno2, deposited using DC Magnetron
Sputtering on Si substrate with Gold Electrodes ?





Rahul Mishra
Research Student (M.Sc.(Engg))
Department of Instrumentation
IISc, Bangalore-560012
Ph. : 394 2349
==============================
Students' Hostel, E-67
Ph. : 394 2622

[email protected]
[email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group