MEMSnet Home: MEMS-Talk: thick aluminum film on wafers
thick aluminum film on wafers
2002-10-07
[email protected]
2002-10-08
Neal Ricks
2002-10-08
Michele Migliuolo
2002-10-08
Renie Duvall
thick aluminum film on wafers
Renie Duvall
2002-10-08
What diameter,type and qty of wafers? And which type of Al are you looking
for?
Aluminum PVD Pure
Aluminum/1% Silicon
Aluminim/2% Silicon
Aluminum/1% Siliocn/0.5% Copper
Aluminum/1% Silicon/1.0% Copper
Aluminum/1% Silicon/2.0% Copper
Aluminum/0.5% Copper
Aluminum/1.0% Copper
Aluminum/2.0% Copper
Aluminum/4.0% Copper
Aluminum/1% Silicon/0.15% Titanium

On Mon, 7 Oct 2002 15:37:49 -0500 (CDT) [email protected]
wrote:

> Hi all.  I am trying to find a company that
> either supplies silicon wafers
> coated with a thick film of aluminum (2-10
> micron) or one that will do
> electroplating and chemical-mechanical
> polishing to achieve a thick aluminum
> film with surface roughness minimized.  All the
> aluminum plated wafers I've
> found have had very thin films (



1-360-263-8011


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering