etching Si-N, but not Al2O3
2002-10-21
Honggang Jiang
etching Si-N, but not Al2O3
Honggang Jiang
2002-10-21
Hi,
I wonder if somebody can suggest any etchants that
etch PECVD Si-N, but do not etch or etch very slowly
alumina coating. Thanks in advance for your help

Honggang Jiang
Second Sight, LLC
28460 Avenue Stanford, Suite 200
Valencia, California 91355
Ph: 661 775 3990
Fx: 661 775 3989

__________________________________________________
Do you Yahoo!?
Y! Web Hosting - Let the expert host your web site
http://webhosting.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review