MEMSnet Home: MEMS-Talk: Re: Glass to Glass Bonding Service
Re: Glass to Glass Bonding Service
RE: stiction of contacting surfaces
2002-10-15
黄树森
2002-10-22
Yuebin Ning
Re: Glass to Glass Bonding Service
Yuebin Ning
2002-10-22
Dlee:

Norcada is a MEMS R&D service company with experience in fabrication of
microfluidic devices. Norcada usually takes on the full fabrication of the
required microfluidic devices, but can consider offering glass - glass
bonding service as well.  You can contact us to discuss your requirement in
detail, and hope we can offer the service you need.

Yuebin Ning, Ph.D.
VP R&D
Norcada Inc
#3, 9808-47 Ave
Edmonton, Canada T6E 5P3
(780)431-9637

> From: "Dlee Li" 
> To: [email protected]
> Date: Fri, 11 Oct 2002 22:43:12 +0000
> Subject: [mems-talk] glass-glass bonding service
> Reply-To: [email protected]
>
> hi, mems researchers
> I am looking for glass-glass bonding services. My material is Pyrex7740.If
> you have such kind of information, please let me know.
>
> thanks in advances!
> Dlee



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
University Wafer