green gold
2002-10-21
Madanagopal K.V.
2002-10-22
sp
2002-10-24
Sivan Lachman Shalem
green gold
sp
2002-10-22
Madan,

I've seen green gold on very thin films ( 50A). It may be that the sticking
coefficient was low due to contamination. Can you see through the green
areas
of the film? It may be that the film is not continuous in that area also due
to
contamination.

                                                Steve
----- Original Message -----
From: "Madanagopal K.V." 
To: 
Sent: Monday, October 21, 2002 11:43 AM
Subject: [mems-talk] green gold


> Hi,
> We evaporated about 50nm gold onto glass substrates.  Some greenish spots
> are seen on parts of the film.  Has anyone seen it before?
>
> Thanks
> Madan
>
> ___________________________________________________________
>
> K.V.Madanagopal, Ph.D.
> Senior Research Associate
> Alliance for Nanomedical Technologies
> 317 Stocking Hall
> Cornell University
> Ithaca
> NY 14850
> Fax:607-255-8741
> Phone:607-254-8052
> ___________________________________________________________
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review