MEMSnet Home: MEMS-Talk: Diffusion barrier for Cr/Au or Ti/Au
Diffusion barrier for Cr/Au or Ti/Au
2002-10-22
Xing Yang
2002-10-23
Neal Ricks
2002-10-23
Simone Capecchi
2002-10-24
Niels Olij
2002-10-24
lakshmikanth namburi
Diffusion barrier for Cr/Au or Ti/Au
Xing Yang
2002-10-22
In Au metalization process, the common adhesion layer Cr or Ti
tends to diffuse through the Au layer, especially at high
temperatures. A quick Google search shows that Pt or Pd has
been commonly used as the diffusion barrier layer. I wonder if
anyone has done any experiments or know any published papers
on this topic. I am looking for information on what the diffusion
barrier layers and their thicknesses have been tried and how
effective they are.

Any info will be appreciated.

Xing Yang




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Addison Engineering
Harrick Plasma, Inc.