Yanjun(David) Tang
2002-10-23
Hi,folks
I'm trying to measure the mechanical properties of silicon dioxide
microcantilever, such as spring constant, resonant frequency, etc. The geometry
of cantilever is about 200*150*1micron. Do you have suggestions about how to do
the job? What kinds of instruments are needed?  I heard that AFM can be used to
measure. I just don't know how? Any opinions will be appreciated. Thanks.

Best regards

Yanjun(David) Tang

Graduate student
Institute for Micromanufacturing
Louisiana Tech University

1401 Tech Farm Rd. Apt. #238, Ruston, LA 71270, USA
Email: [email protected]
          [email protected]

Tel: 1-318-255-5133

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing