Electroless Ni on Au
Peter & Judy Wright
2002-10-30
Is it possible to plate electroless Ni on Au? I have exposed gold pads, in
openings in a silicon nitride passivation layer, which I want to bump. I
would like to use Ni as the UBM and electroless deposition would save me a
photolithography step. If it is possible, what is the chemistry that is
required to catalyze the reaction and will the Ni film adhere well to the
Au?

Thanks for any help.
Peter Wright

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing