MEMSnet Home: MEMS-Talk: Density of gold
Density of gold
2002-11-01
Wayne Seguin
2002-11-04
Christopher F. Blanford
Density of gold
Wayne Seguin
2002-11-01
The Materials list for Material: Gold (Au), bulk shows a Density of 19280
kg/m^3, but I've found many other references that claim the Density is 19320
kg/m^3. (one example: http://www.stanford.edu/~yueliang/constant.htm)
Does anyone know what the difference is between the two? (please don't say
40kg).
Thanks
Wayne