Rough edges in wet etch
foo foo
2002-12-03



dear all

I am etching a thin gold layer about 10-30nm thick with a wet etch, KI. I am
using PMMA polymer as an etch mask. My problem is that I get very rough
edges, by that I mean uneven edges, on the metal after the etching. Does
anyone have any ideas why this happens.

Regards
Patrick

_________________________________________________________________
Hela veckans väder  http://www.msn.se/vader


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer