MEMSnet Home: MEMS-Talk: Photoresists for Hot Phos. Acid Nitride Etching
Photoresists for Hot Phos. Acid Nitride Etching
2002-12-03
Jeff Jessing
2002-12-04
Roger Brennan
2002-12-06
[email protected]
Photoresists for Hot Phos. Acid Nitride Etching
[email protected]
2002-12-06
Photoresists do not hold up to hot phosphoric reflux etching. It is typical to
plasma etch nitride and then remove the patterned nitride without photoresist at
a later step. Bob Henderson

reply