polyimide etching
1997-05-14
Ralf Keller
polyimide etching
Ralf Keller
1997-05-14
I try to etch polyimide (DuPont Pyralin 2611) in a O2-plasma (RIE) and I
always get some residue on the wafer.
Does anybody know how to solve this problem ?

Thanks in advance,

Ralf

****************************************
Dipl. Ing. (FH) Ralf Keller

Fraunhofer-Institut fuer Biomedizinische Technik
Fraunhofer Institute for Biomedical Engineering
Ensheimer Str. 48
66386 St. Ingbert, Germany
Tel.: +49 (0) 6894 / 980-158     Fax: ..-400
e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing