MEMSnet Home: MEMS-Talk: Re: Protective coating for KOH etch
Re: Protective coating for KOH etch
1997-05-17
Bin Yuan
1997-05-19
[email protected]
Re: Protective coating for KOH etch
Bin Yuan
1997-05-17
Black wax (Apiezon) is the protective coating that we have used. It can be
dissolved by xylene or trichloroethylene.

Good luck.

Bin Yuan
Department of Mechanical Engineering
The Johns Hopkins University
Baltimore, MD 21218
(410) 516-6665

On Fri, 9 May 1997, James R. Stackhouse wrote:

> We are trying to use KOH to place a 5 micron deep etch on one side of
> silicon wafer, and 25 micron on other side.  We are looking for a
> protective coating we could apply to one side of the wafer after we've
> done the first 5 microns of the etch, then continue with the final etch
> on the other side.  Can anyone suggest a solution to this two step etch
> process ?  Possibly a spin-on layer to be removed after the etching ?
>
> Thanks,
> Jim Stackhouse
> Phil Klauder
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.