Glass-Glass Direct Bonding
2002-12-17
Helen Li
Glass-Glass Direct Bonding
Helen Li
2002-12-17
Hi All,

I am trying the glass-glass direct bonding on my wafer
(silicate glass). I
read about the precess consisting of

(1) hydrphilization: with H2SO4:H2O2, or
H2O2:NH4OH:H2O
(2) bonding: light pressaure applied in the center of
the wafer, achieve
        bonding across the whole wafer at room
temperature
(3) annealing: 350 deg C for hours to stabilize the
bonding

I tried but failed. Does anyone have success in
glass-glass direct
bonding? My questions are:
what is the ratio of the mixture for hydrophilization?
Is that very critical?
What is the proper pressure to apply?
Has any one achieve the bonding using EV bonder? Can
you tell me some more
about the process? Does the wafer size and thickness
matter?

Thanks so much for your help.

Best,
Helen



__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
MEMStaff Inc.
MEMS Technology Review