Dear all:

I want to etch silicon wafer with Tungsten as mask to make a 1um deep trench. We
don't want undercut happen, so we need to find a anistropic etchant for silicon.
Would anyone can provide me some suggestion about the anistropic etchant in this
case? Your help is greatly appreciated.

Have a nice holiday,


changhong

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing