MEMSnet Home: MEMS-Talk: Shipley1813 on su-8
Shipley1813 on su-8
2002-12-17
Soojin Oh
Shipley1813 on su-8
Soojin Oh
2002-12-17
I spin-coated su8 25 on my ITO wafer and after soft
bake (as instructed by MicroChem) I spin-coated S1813
on it and baked it at 95C briefly. At this stage the
two layers of photoresist look fine. But after UV
exposure (330 um 20 sec), it was apparent that
something's happened on the second PR or interface
btwn S1813 and su8. To describe the apperance it looks
like the surface of the Moon under microscope! Some
bumpy bubble-like stuffs all over the surface. Can
anybody explain what I did? Thank you.


__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review