How to fabricate W and Mo
Mighty Platypus
2002-12-26
Greetings, Tae-Won,
According to a metal etchants sheet I have:

Mo -> HCl:H2O2 1:1
W  -> HF:HNO3  1:1

should work at room temperature. I don't have etch rates.

If you can find a copy of the CRC Handbook of Etchants for Metals and
Metallic Compounds, It's pretty good.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Never worry again about the quality of your random numbers!"
    -- Advertisement

On Thu, 26 Dec 2002, Lee Tae-Won wrote:

> Dear colleagues.
>
> I'm trying to etch sputtered Mo and W after photo-lithography.
>
> Could you please let me know which wet&dry etchants are effective for these
materials.
>
> furthermore  , Adhesion ability with Au(gold) is good in these materials?
>
> Thank you for your help , in advance.
>
>
> PS .  Recommendation  of related references and papers would be appreciated.
>
> E-mail : [email protected]
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing