MEMSnet Home: MEMS-Talk: Uniform Teflon coating on Parylene C
Uniform Teflon coating on Parylene C
2002-12-26
Richard Chen
2002-12-31
Richard Chen
2003-01-08
Mighty Platypus
Uniform Teflon coating on Parylene C
Mighty Platypus
2003-01-08
Hello Richard,
I've had quite a bit of experience with spinnable teflon. Can you describe
the nonuniformity in some more detail, and tell me which type of teflon AF
you are using, as well as which type of Parylene-C, process details, etc?

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Never worry again about the quality of your random numbers!"
    -- Advertisement

On Tue, 31 Dec 2002, Richard Chen wrote:

> Hi,
> Does anyboby know how to spin coat a uniform Teflon coating on Parylene C? I
> had tried many times, however, the coating was so nonuniform. If you know
> how to make it more uniform and better adhesive to the Parylene C, please
> reply. Thanks a lot.
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review