MEMSnet Home: MEMS-Talk: Pin holes in Pt
Pin holes in Pt
2003-01-10
jiaz
2003-01-28
张振峰
Pin holes in Pt
jiaz
2003-01-10
Hi, there.

In our experiments, on the surface of the sputtered Ti/Pt(on top of
SiO2), many pin holes came out after the annealing for the metals at
650C, 30min. Who can kindly tell me the reasons and the solution will be
really appereciated.

Looking forward to your help.

********************************************************************
Zhou, Jia
Center of Microtechnologies, Chemnitz University of Technology
Reichenhainer Street 88, RM. M211
D-09126, Chemnitz, Germany
********************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
MEMS Technology Review
MEMStaff Inc.