Dear Colleagues,

Am searching for practical information / experience on sputtering metallization.
I'm using SOI wafers and i tried to have Cr/Pt/Au contacts on Si. After
sputtering, I did a post bake and I had a long HF 48% attack. It look like an
etch under contacts.
Does anybody know this problem and how to avoid it?
Any experiences, information, recipes, etc would be greatly appreciated.

Best regards,

Benoît GAULIER.

--
=================================================
   Benoît GAULIER
   Ingénieur Filière Microtechnologie
   THALES AVIONICS
   NAVIGATION
   25, rue Jules Védrines 26027 Valence CEDEX
   Télécopie: (+33) (0) 4-75-79-86-06
   Bureau: (+33) (0) 4-75-79-88-25
=================================================



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.