A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Seperating plated copper from a silicon mould
Seperating plated copper from a silicon mould
2003-01-23
Cormac Eason
Seperating plated copper from a silicon mould
Cormac Eason
2003-01-23
Hi all,

I'm currently investigating processes for making microchannels by Electroplating
copper. One method I came across used a silicon mould which was then plated over
by copper to form a copper block with the inverse of the mould geometry on its
surface.

I'm wondering how the copper was seperated from the silicon. Is there a layer or
surface treatment which can be used? If a photoresist is being used, is there a
standard method available to coat it evenly over the mould before the seed layer
is evaporated on? Can a reasonably even layer be deposited by dipping the mould
in resist and leaving excess resist to drip off before baking?

All help would be greatly appreciated.

Regards,

Cormac Eason.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
MEMS Technology Review
Tanner EDA by Mentor Graphics