A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Etching Si with SiO2 as mask
Etching Si with SiO2 as mask
2002-11-25
Patrick Carlberg
2002-11-25
Hsu-Wei Fang
2002-11-25
Robert Dean
2002-11-25
Hongjun Zeng
2002-11-25
foo foo
2002-11-25
Knighton, Ed
2002-11-27
Beverley Eyre
2002-11-26
Burkhard Volland
Etching Si with SiO2 as mask
Hongjun Zeng
2002-11-25
RIE with SF6 etches si much faster that it etches SiO2.

Good luck,

Hongjun Zeng, Ph.D
Microfabrication Applications Laboratory (MAL)
University of Illinois at Chicago
ERF Building, 842 W. Taylor Street
Chicago, IL 60607-7022
Room 3014 ERF
Tel.: 312-413-5889, Fax: 312-996-6465

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Patrick Carlberg
Sent: Monday, November 25, 2002 8:48 AM
To: [email protected]
Subject: [mems-talk] Etching Si with SiO2 as mask


Dear all

I am interesseted in etching Si with SiO2 as an etch mask. Does anyone
know of a dry or wet etch that can be used?

All comments are highly apriciated

Patrick





_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.