MEMSnet Home: MEMS-Talk: nickel as a mask in EDP
nickel as a mask in EDP
2003-02-03
Prem Pal
2003-02-03
Dan.W.Chilcott
2003-02-03
[email protected]
2003-02-04
[email protected]
nickel as a mask in EDP
Dan.W.Chilcott
2003-02-03
Prem Pal-
I have used nickel for a mask in EDP and KOH.The nickel is not attacked
but at least in KOH an oxide was formed.If you need to remove the nickel
after the etch you may have a problem. I used sputtered nickel.

Dan Chilcott

-----Original Message-----
From: Prem Pal [mailto:[email protected]]
Sent: Monday, February 03, 2003 6:48 AM
To: [email protected]
Subject: [mems-talk] nickel as a mask in EDP


Dear all
Can electroless or electroplated Nickel be used as a mask for
anisotropic etching in EDP.any type of suggetion would be highly
appreciated.
thanx


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing