adnan merhaba
Ni-Cr and Si-Cr sputtering
adnan merhaba
2003-02-07
Dear MEMS Colleagues,

I have a couple of questions:

1. Can anyone provide me with information regarding
target composition and sputtering parameters for Ni-Cr
(RF and DC) to achieve a TCR < 50ppm.

2. I am also experimenting with Si-Cr (to achieve high
value resistors), does anyone have any experience with
sputter deposition (DC and RF) of this material?

Thank you,
Regards,
Adnan Merhaba

__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group