Removing PDMS
2003-02-12
Christabel Tan
2003-02-12
[email protected]
Removing PDMS
[email protected]
2003-02-12
I have worked with Cris Meiners group at U of M and they claim that Dynasolve
will remover RTV which is a form of PDMS.  You can treat your wafers with
methyltrichlorosilane vapor to prevent adhesion of PDMS.
Scott


reply