MEMSnet Home: MEMS-Talk: my Pyralin is breaking off
my Pyralin is breaking off
2003-02-13
Yair
2003-02-17
Rivas, Isabel
2003-02-19
Yair
2003-02-20
Rivas, Isabel
my Pyralin is breaking off
Yair
2003-02-13
Hello,
I'm using Pyralin 2555 (1:1), ~3um thick, as a dielectric thin film.
After photolitogrphy and development, I want to remove the photoresist
(AZ2020) with Acetone, but the Pyralin is peeling off my substrate as
well (it is not cured yet). Can anyone recommend me something about
that?
Thanks a lot,

Yair Gannot, Process Engineer
Wolfson Microelectronics Research Center
TECHNION - ISRAEL INSTITUTE OF TECHNOLOGY
Technion City, Haifa 3200, Israel
Tel- +972-4-8293291

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation