probs removing S1813 from glass after E-beam evap
2003-02-13
Timothy D. Meehan
2003-02-18
Sang (Kevin) Kim
probs removing S1813 from glass after E-beam evap
Timothy D. Meehan
2003-02-13
I am having difficulty doing lift-off of Shipley 1813 resist from glass
following electron beam evaporation of Ti/Au. The evaporation follows
standard photolithographic UV exposure and developing. The lift-off
protocol I am using is sonication in acetone. Out of frustration I have
even soaked the sample in nanostrip for an hour to no avail. Any advice
would be appreciated.



Tim Meehan
Superfine Group
Department of Chemistry
University of North Carolina
@ ChapelHill


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.