A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: General Book on Etchants
Re: General Book on Etchants
1997-06-26
Shekhar Bhansali
Re: General Book on Etchants
Shekhar Bhansali
1997-06-26
The CRC handbook of metal etchants is one of the the most comprehensive
references for etchants.  It is available from CRC Press cleveland Ohio.

The contact details and the price (inJan 97) are hereunder:
           "CRC Handbook of Metal etchants"
          The above title is available at $300.00 US plus $35.15 for
          shipping and handling via Federal Express (daytime number is
          necessary) or by airmail, the shipping cost would be $45.25.

          Prepayment is required.  We accept Visa, Mastercard, and
          American Express.

          Best regards,

          Debby Cabel
          International Customer Service Rep.
          CRC Press LLC

          Fax #561-989-8732
          e-mail:[email protected] (Cabel, Debby)

Shekhar Bhansali

>Can anyone recommend a general book on etch recipies for RIE, plasma, and/or
>wet chemical?
>                                        Justin.
>Justin D. Mansell                | "If your opponent strikes with fire,
>Ginzton Laboratory               |          counter with water."
>Stanford, CA 94305               | "A true warrior is invincible because
>tel: 415-725-2266                |          he contests with nothing."
>fax: 415-723-2666                | "To injure an opponent is to injure
>yourself."
>http://www.stanford.edu/~jmansell|                              -Morihei
>Ueshiba
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search