sou zou
2003-02-18
Hi folks,

The stiction for MEMS due to damp is not a new behaviour. In fact, we are
getting in trouble to move our devices (MUMP's components, but Before we didn't
get this problem). So, we are expecting a high level of damp in the experiment
area in use. My concern is how to tackle this prb immediately (e.g by using a
special spray or stuff like that ?).

Many thanks,

Sofiane



---------------------------------
Do You Yahoo!? -- Une adresse @yahoo.fr gratuite et en français !
Testez le nouveau Yahoo! Mail
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.