Photosensitive Parylene?
Bill Moffat
2003-03-05
Steve,
      Photosensitive Polymide and BCB exist which after the correct bake have
equivalent qualities to Parylene.  Bill Moffat

-----Original Message-----
From: Hovey, Steve [mailto:[email protected]]
Sent: Tuesday, March 04, 2003 9:16 AM
To: '[email protected]'
Subject: [mems-talk] Photosensitive Parylene?


Hi.  This is my first posting to this mailing list.

I was wondering if anyone out there had ever heard of such a thing as
photosensitive Parylene?  I'm not sure how one would go about producing such
a thing, but if it were possible, the applications would be extensive.

Thanks,  Steve

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group