Re: about growth of SiN layer on porous silicon?
2003-03-24
高 晓童
Re: about growth of SiN layer on porous silicon?
高 晓童
2003-03-24
Dear All,

    Thank you, Marc! But what I am concerned is how to grow a SiN layer on
a porous silicon layer, not in the pores. The papers you gave me is about
the later issue.

    Who can give me some information about my issue? Thank you in advance!

Best regards,

Xiaotong Gao


>Dear MEMS-Colleagues,
>
>Yes, there have been studies on the growth of a nitride layer on porous
si=
>licon (macroporous silicon). The work has been done in Dr. Lehmann's
group=
>, see e.g., V. Lehmann, W. Honlein, H. Reisinger, A. Spitzer, H. Wendt,
J.=
> Willer, Thin Solid Films, 276, 138, 1996, or: LEHMANN, V., R=D6NNEBECK,
S.,=
> Sensors and Actuators A, 95, 202 (2001). These Si3N4 have an excellent
qu=
>ality.
>
>I hope this helps. If you need more information, send me an email.
>
>With best regards
>   Marc
>
>
>Marc Christophersen, PhD      =20
>University of Rochester, NY=20
>601 Elmwood Ave. =20
>P.O. Box CFH =20
>Rochester, NY 14642 US =20
>http://marc-christophersen.de






_________________________________________________________________
享用世界上最大的电子邮件系统― MSN Hotmail。  http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
The Branford Group